Présentation:
Stainless steel wire is fabricated from an iron alloy that offers high resistance to corrosion, including staining and rusting, in many environments where spring or galvanized steel wire would typically degrade. Its performance properties, including corrosion resistance and strength, depend on its numerical grade. Type 304 stainless steel wire, also known as 18-8, is a general-purpose material that combines corrosion resistance, weldability, and formability, making it the most commonly used grade of stainless steel. The 316 stainless steel wire grade provides increased corrosion resistance compared to 304. Stainless steel wire is typically uncoated, and may have a specific finish such as bright or mirror indicated. Temper is available in two forms: soft and spring. Spring stainless steel wire is able to retain its shape after bending, while the soft temper typically maintains its bent position.
Caractéristiques:
1. High conductivity
2. Shock resistance
3. Excellent durability
4. Superior strength
5. Rust resistant
6. Low maintenance
7. Affordability
8. Durable Finish
9. Corrosion Resistant
10. Reliability
11. Resistance to heat
Spécifications:
Note: Special size and specifications can be made according to customers requires.
Technologie:
AISI material | Chemical compositions (%) | |||||||
C | Si | Mn | P | S | Ni | Cr | Mo | |
304 | =<0.08 | =<1.00 | =<2.00 | =<0.045 | =<0.030 | 8.00~10.50 | 18.00~20.00 | - |
304H | >0.08 | =<1.00 | =<2.00 | =<0.045 | =<0.030 | 8.00~10.50 | 18.00~20.00 | - |
304L | =<0.030 | =<1.00 | =<2.00 | =<0.045 | =<0.030 | 9.00~13.50 | 18.00~20.00 | - |
316 | =<0.045 | =<1.00 | =<2.00 | =<0.045 | =<0.030 | 10.00~14.00 | 10.00~18.00 | 2.00~3.00 |
316L | =<0.030 | =<1.00 | =<2.00 | =<0.045 | =<0.030 | 12.00~15.00 | 16.00~18.00 | 2.00~3.00 |
430 | =<0.12 | =<0.75 | =<1.00 | =<0.040 | =<0.030 | =<0.60 | 16.00~18.00 | - |
430A | =<0.06 | =<0.50 | =<0.50 | =<0.030 | =<0.50 | =<0.25 | 14.00~17.00 | - |
Désignation de Produit: Fil d'acier inoxydable